Description :
Tenders for Supply Of Pig Iron With Chemical Composition As: Carbon : 3.5% To 4.6%, Silicon : 1.00% (max), Man Ganese : 1.0% (max), Sulphur :0.060% (max), Phosphorus :0.110% (max), Iron (fe): 92% (min). Note: (1) We Ight Of Pig Iron Ingots Should Be In Range From 3.5 Kg To 45 Kgs. (2) Other Elements Like Cu, Ni, Cr, Mo, Sn, Pb, Zn, V Etc. Can Be Permitted In Traces Only. (3) Sampling, Inspection And Testing Of Pig Iron Shall Be Done In Line With Is-13502:2023 Or Latest. [ Warranty Period: 12 Months After The Date Of Delivery ]